Osprey® 90

SuperalloyDatasheet

Powder designed for

  • Additive Manufacturing
  • Metal Injection Moulding (MIM)

Standards

  • UNS N07090
  • EN Number 2.4632
  • EN Name NiCr20Co18Ti

Datasheet updated Apr 6, 2023 6:45 AM CET (supersedes all previous editions)

Disclaimer: Data and recommendations are for guidance only, and the suitability of a powder for a specific process or application can be confirmed only when we know the actual conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Osprey® powder.

Osprey® 90 is an age-hardenable creep-resistant nickel-chromium-cobalt superalloy characterized by good resistance to high-temperature corrosion and oxidation. The alloy is typically used for aerospace applications. Osprey® 90 is an alloy of the same type as Nimonic® 90*.

Osprey® metal powder is manufactured by Inert Gas Atomization (IGA), producing a powder with a spherical morphology which provides good flow characteristics and high packing density. In addition, the powder has a low oxygen content and low impurity levels, resulting in a metallurgically clean product with enhanced mechanical performance.

*Nimonic® 90 is a trademark owned by Special Metals.

Chemical composition (nominal), %
Ni Fe C Cr Al Ti Other
Bal. ≤1.5 ≤0.13 20.0 1.0-2.0 2.0 Co 18.0

Disclaimer: Data and recommendations are for guidance only, and the suitability of a powder for a specific process or application can be confirmed only when we know the actual conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Osprey® powder.