Superalloys

The standard range of Osprey® metal powder includes a wide variety of nickel-based superalloys to be used in, for example, additive manufacturing and metal injection moulding (MIM).

Need to know more?

Call us Email us

Other superalloys are also available. Contact us to discuss our full range of metal powder alloys.

Ni-based superalloys

Our nickel-based superalloys are used in a range of applications where high-temperature corrosion and oxidation resistance are key attributes. Examples are jet turbines, gas turbines, oil and gas, pressure vessels or chemical processing components.

Our range of nickel superalloys includes, for example, the below grades. Several of the grades are widely used in additive manufacturing. Read more about Ni-based superalloys for additive manufacturing

Selected superalloys incl. chemical composition (nominal), %
Alloy (UNS) Description Ni Fe C Cr Mo Al Ti Nb Other
625
(N06625)
See below1) 58.0 min ≤5 ≤0.1 20.0-23.0 8.0 – 10.0 ≤0.4 ≤0.4 3.15–4.15 -
713C See below2) Bal. ≤2.5 0.08-0.20 12.0-14.0 3.8-5.2 5.0-6.5 0.5-1.0 1.8-2.8 B 0.05-0.15
Zr 0.05-0.15
718
(N07718)
See below3) 50.00-55.00 Bal. ≤0.08 17.00-21.00 2.80-3.30 0.20-0.80 0.65-1.15 4.75-5.50 -
90
(N07090)
See below4) Bal. ≤1.5 ≤0.13 20.0
-
2 2.0
-
Co 18.0
H-X
(N06002)
See below5) Bal. 19 ≤0.15 21.0 9.0
-
-
-
Co 1.0

1) This alloy resists a wide range of severely corrosive environments.
2) This alloy combines excellent fatigue resistance and rupture strength at high temperature.
3) This alloy combines corrosion resistance and high strength with outstanding weldability including resistance to post-weld cracking.
4) This alloy also has good resistance to high-temperature corrosion and oxidation.
5) This alloy is used extensively in high-temperature applications.

Price and delivery