Superalloys
The standard range of Osprey® metal powder includes a variety of Ni-based superalloys for use in, for example, Additive Manufacturing (AM), cold spray, Hot Isostatic Pressing (HIP) and Metal Injection Moulding (MIM).
| Osprey® | Standards* | Ni | Fe | C | Cr | Mo | Al | Ti | Nb | Co | B | Mn | Si | P | S | Other | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 625 | UNS N06625 | 58.0 min | ≤5.0 | ≤0.1 | 20.0-23.0 | 8.0-10.0 | ≤0.4 | ≤0.4 | 3.15-4.15 (Nb+Ta) | ≤1.0 | - | ≤0.5 | ≤0.5 | ≤0.015 | ≤0.015 | - |
625
|
| 713C | UNS N07713 | Bal. | ≤2.5 | 0.08-0.20 | 12.0-14.0 | 3.8-5.2 | 5.0-6.5 | 0.5-1.0 | 1.8-2.8 | - | 0.05-0.15 | - | - | - | - | Zr 0.05-0.15 |
713C
|
| 718 | UNS N07718 | 50.0–55.0 | Bal. | ≤0.08 | 17.0-21.0 | 2.80-3.30 | 0.20-0.80 | 0.65-1.15 | 4.75-5.50 | ≤1.00 | ≤0.006 | ≤0.35 | ≤0.35 | ≤0.015 | ≤0.015 | Cu ≤0.30 |
718
|
| 80A | UNS N07080 | Bal. | ≤3.0 | ≤0.10 | 18.0-21.0 | - | 1.0-1.8 | 1.8-2.7 | - | ≤2.0 | ≤0.008 | ≤1.0 | ≤1.0 | - | ≤0.015 | Cu ≤0.2, Zr ≤0.15, Pb ≤0.003 |
80A
|
| 90 | UNS N07090 | Bal. | ≤1.5 | ≤0.13 | 20.0 | - | 1.0-2.0 | 2.0 | - | 18.0 | - | - | - | - | - | - |
90
|
| H-X | UNS N06002 | Bal. | 18 | ≤0.15 | 21.0 | 9.0 | - | - | - | 1.0 | ≤0.008 | ≤0.1 | ≤0.1 | ≤0.015 | ≤0.015 | W 0.7 |
H-X
|
* Information about more standards is available in the datasheet for the respective alloy.