Jump to content
Back to Superalloys

Osprey® 713C

Superalloys

Osprey® 713C

Osprey® 713C is a precipitation hardenable nickel-chromium superalloy with excellent resistance to oxidation and thermal fatigue resistance as well as high rupture strength and structural stability at high temperature.

UNS
N07713
EN Name
2.4856
SAE
AMS5377

Powder designed for

  • Additive Manufacturing (AM)
  • Metal Injection Moulding (MIM)

This metal powder is manufactured by Inert Gas Atomization (IGA), producing a powder with a spherical morphology which provides good flow characteristics and high packing density.

Technical data

Page updated Sep 18, 2023 11:03 AM CET (supersedes all previous editions)

  • Chemical composition (nominal), %

    Ni
    Bal.
    Fe
    ≤2.5
    C
    0.08-0.20
    Cr
    12.0-14.0
    Mo
    3.8-5.2
    Al
    5.0-6.5
    Ti
    0.5-1.0
    Nb
    1.8-2.8
    B
    0.05-0.15
    Other
    Zr 0.05-0.15
  • Powder characteristics and morphology

    Powder for Additive Manufacturing

    Osprey® metal powder for Additive Manufacturing is characterized by a spherical morphology and high packing density, which confer good flow properties. For powder bed processes these are essential when applying fresh powder layers to the bed to ensure uniform and consistent part build.

    For blown powder processes, such as Direct Energy Deposition (DED), good flow ensures uniform build rates. Tight control of the particle size distribution also helps ensure good flowability. Low oxygen powders result in clean microstructures and low inclusion levels in the finished parts.

    The powder morphology of Osprey® nickel-based alloy powder is typically spherical, with smooth surface and low level of powder satellites.

    Powder for Metal Injection Moulding (MIM)

    Osprey® MIM powder has a spherical morphology, resulting in high packing density. This enables the manufacture of feedstocks with high powder loading, which not only minimizes binder costs but also reduces part shrinkage during debinding and sintering. Spherical powder also has excellent flow characteristics, resulting in reduced tool wear and consistent mould filling.

    Osprey® MIM powder's low oxygen content allows better control of carbon and consistency during sintering. Low oxygen levels, together with high packing density, also facilitate faster sintering.

  • Particle size distribution

    Powder for Additive Manufacturing

    Osprey® metal powder for Additive Manufacturing is available in a wide range of particle size distributions that are tailored to the individual Additive Manufacturing systems. They can also be tailored to the particular requirements of the end application, both in terms of mechanical performance and surface finish.

    Typical particle size distributions for Additive Manufacturing.

    Typical particle size distributions for Additive Manufacturing
    Process technology Size (µm)
    Binder jetting ≤ 16, ≤ 22, ≤ 32, ≤ 38, ≤ 45
    Laser - Powder Bed Fusion (L-PBF) 15 to 53 and 10 to 45
    Electron beam - Powder Bed Fusion (E-PBF) 45 to 106
    Direct Energy Deposition (DED)

    53 to 150

    Powder for Metal Injection Moulding (MIM)

    Osprey® metal powder for Metal Injection Moulding (MIM) is available in a wide range of particle size distributions, from under 5 μm up to 38 μm. The table shows our standard particle size distributions for MIM powders.

    Typical particle size distributions for Metal Injection Moulding (MIM)*
    Size (μm) D10 (μm) D50 (μm) D90 (μm)
    ≤ 38 5.5 13.0 31.0
    ≤ 32 5.0 12.0 29.0
    80% ≤ 22 4.5 11.5 27.0
    90% ≤ 22 4.0 10.5 22.0
    90% ≤ 16 3.5 8.0 16.0

    *Particle size measurements performed using a Malvern laser particle size analyzer, typical D10, D50 and D90 provided.

    Tailor-made particle size distributions are available on request. Contact us to discuss your specific requirements.

  • Testing

    All Osprey® metal powders are supplied with a certificate of analysis containing information on the chemical composition and particle size distribution. Information on other powder characteristics is available upon request.

  • Packaging

    A wide range of packaging options are available, from 1 kg (2.2 lb) to 200 kg (440 lb)*.

    Contact our team who can support you with selecting the right packaging for your product and application.

    *Some packaging options may not be available for all products due to international shipping regulations.

Disclaimer: Data and recommendations are for guidance only, and the suitability of a powder for a specific process or application can be confirmed only when we know the actual conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Osprey® powder.

Range of superalloys

Osprey® Standards* Ni Fe C Cr Mo Al Ti Nb Co B Mn Si P S Other
625 UNS N06625 58.0 min ≤5.0 ≤0.1 20.0-23.0 8.0-10.0 ≤0.4 ≤0.4 3.15-4.15 (Nb+Ta) ≤1.0 - ≤0.5 ≤0.5 ≤0.015 ≤0.015 - 625
713C UNS N07713 Bal. ≤2.5 0.08-0.20 12.0-14.0 3.8-5.2 5.0-6.5 0.5-1.0 1.8-2.8 - 0.05-0.15 - - - - Zr 0.05-0.15
718 UNS N07718 50.0–55.0 Bal. ≤0.08 17.0-21.0 2.80-3.30 0.20-0.80 0.65-1.15 4.75-5.50 ≤1.00 ≤0.006 ≤0.35 ≤0.35 ≤0.015 ≤0.015 Cu ≤0.30 718
80A UNS N07080 Bal. ≤3.0 ≤0.10 18.0-21.0 - 1.0-1.8 1.8-2.7 - ≤2.0 ≤0.008 ≤1.0 ≤1.0 - ≤0.015 Cu ≤0.2, Zr ≤0.15, Pb ≤0.003 80A
90 UNS N07090 Bal. ≤1.5 ≤0.13 20.0 - 1.0-2.0 2.0 - 18.0 - - - - - - 90
H-X UNS N06002 Bal. 18 ≤0.15 21.0 9.0 - - - 1.0 ≤0.008 ≤0.1 ≤0.1 ≤0.015 ≤0.015 W 0.7 H-X

* Information about more standards is available in the datasheet for the respective alloy.

For more information

Get in touch with our experts in metal powder today

We would like your consent

Sandvik and our vendors use cookies (and similar technologies) to collect and process personal data (such as device identifiers, IP addresses, and website interactions) for essential site functions, analyzing site performance, personalizing content, and delivering targeted ads. Some cookies are necessary and can’t be turned off, while others are used only if you consent. The consent-based cookies help us support Sandvik and individualize your website experience. You may accept or reject all such cookies by clicking the appropriate button below. You can also consent to cookies based on their purposes via the manage cookies link below. Visit our cookie privacy policy for more details on how we use cookies.