Osprey® H-X
Superalloys
Osprey® H-X
Osprey® H-X is a nickel-chromium-molybdenum-iron superalloy characterized by high-temperature strength and good resistance to oxidation.
- UNS
- N06002
- EN Number
- 2.4665
Powder designed for
- Additive Manufacturing (AM)
- Metal Injection Moulding (MIM)
This metal powder is manufactured by either induction melting under Vacuum Inert Gas Atomization (VIGA) or melting under argon prior to Inert Gas Atomization (IGA).
-
Product description
Osprey® H-X is a nickel-chromium-molybdenum-iron superalloy characterized by high-temperature strength and good resistance to oxidation. The alloy is typically used in aerospace, oil and gas applications. Osprey® H-X is an alloy of the same type as Hastelloy® X and Inconel® alloy HX*.
This metal powder is manufactured by either induction melting under Vacuum Inert Gas Atomization (VIGA) or melting under argon prior to Inert Gas Atomization (IGA), producing a powder with a spherical morphology which provides good flow characteristics and high packing density. In addition, the powder has a low oxygen content and low impurity levels, resulting in a metallurgically clean product with enhanced mechanical performance.
*Hastelloy® is a trademark owned by Haynes International Inc. Inconel® is a trademark owned by Huntington Alloys Corporation.
Product description
Osprey® H-X is a nickel-chromium-molybdenum-iron superalloy characterized by high-temperature strength and good resistance to oxidation. The alloy is typically used in aerospace, oil and gas applications. Osprey® H-X is an alloy of the same type as Hastelloy® X and Inconel® alloy HX*.
This metal powder is manufactured by either induction melting under Vacuum Inert Gas Atomization (VIGA) or melting under argon prior to Inert Gas Atomization (IGA), producing a powder with a spherical morphology which provides good flow characteristics and high packing density. In addition, the powder has a low oxygen content and low impurity levels, resulting in a metallurgically clean product with enhanced mechanical performance.
*Hastelloy® is a trademark owned by Haynes International Inc. Inconel® is a trademark owned by Huntington Alloys Corporation.
Osprey® H-X is a nickel-chromium-molybdenum-iron superalloy characterized by high-temperature strength and good resistance to oxidation. The alloy is typically used in aerospace, oil and gas applications. Osprey® H-X is an alloy of the same type as Hastelloy® X and Inconel® alloy HX*.
This metal powder is manufactured by either induction melting under Vacuum Inert Gas Atomization (VIGA) or melting under argon prior to Inert Gas Atomization (IGA), producing a powder with a spherical morphology which provides good flow characteristics and high packing density. In addition, the powder has a low oxygen content and low impurity levels, resulting in a metallurgically clean product with enhanced mechanical performance.
*Hastelloy® is a trademark owned by Haynes International Inc. Inconel® is a trademark owned by Huntington Alloys Corporation.
Technical data
Page updated Jul 19, 2023 10:04 AM CET (supersedes all previous editions)
Downloads
-
Chemical composition (nominal), %
Ni Bal.Fe 18C ≤0.15Cr 21.0Mo 9.0Co 1.0B ≤0.008Mn ≤0.1Si ≤0.1P ≤0.015S ≤0.015Other W 0.7 -
Powder characteristics and morphology
Powder for Additive Manufacturing
Osprey® metal powder for Additive Manufacturing is characterized by a spherical morphology and high packing density, which confer good flow properties. For powder bed processes these are essential when applying fresh powder layers to the bed to ensure uniform and consistent part build.
For blown powder processes, such as Direct Energy Deposition (DED), good flow ensures uniform build rates. Tight control of the particle size distribution also helps ensure good flowability. Low oxygen powders result in clean microstructures and low inclusion levels in the finished parts.
SEM micrographs of Osprey® H-X -53 +15 µm powder with a spherical morphology.
SEM micrographs of Osprey® H-X, a section through the printed Laser - Powder Bed Fusion (L-PBF) material, which notably shows the absence of cracks.Powder for Metal Injection Moulding (MIM)
Osprey® MIM powder has a spherical morphology, resulting in high packing density. This enables the manufacture of feedstocks with high powder loading, which not only minimizes binder costs but also reduces part shrinkage during debinding and sintering. Spherical powder also has excellent flow characteristics, resulting in reduced tool wear and consistent mould filling.
Osprey® MIM powder's low oxygen content allows better control of carbon and consistency during sintering. Low oxygen levels, together with high packing density, also facilitate faster sintering.
-
Particle size distribution
Powder for Additive Manufacturing
Osprey® metal powder for Additive Manufacturing is available in a wide range of particle size distributions that are tailored to the individual Additive Manufacturing systems. They can also be tailored to the particular requirements of the end application, both in terms of mechanical performance and surface finish.
Typical particle size distributions for Additive Manufacturing.Typical particle size distributions for Additive Manufacturing Process technology Size (µm) Binder jetting ≤ 16, ≤ 22, ≤ 32, ≤ 38, ≤ 45 Laser - Powder Bed Fusion (L-PBF) 15 to 53 and 10 to 45 Electron beam - Powder Bed Fusion (E-PBF) 45 to 106 Direct Energy Deposition (DED) 53 to 150
Powder for Metal Injection Moulding (MIM)
Osprey® metal powder for Metal Injection Moulding (MIM) is available in a wide range of particle size distributions, from under 5 μm up to 38 μm. The table shows our standard particle size distributions for MIM powders.
Typical particle size distributions for Metal Injection Moulding (MIM)* Size (μm) D10 (μm) D50 (μm) D90 (μm) ≤ 38 5.5 13.0 31.0 ≤ 32 5.0 12.0 29.0 80% ≤ 22 4.5 11.5 27.0 90% ≤ 22 4.0 10.5 22.0 90% ≤ 16 3.5 8.0 16.0 *Particle size measurements performed using a Malvern laser particle size analyzer, typical D10, D50 and D90 provided.
Tailor-made particle size distributions are available on request. Contact us to discuss your specific requirements.
-
Mechanical properties
Typical mechanical properties of material produced by Laser - Powder Bed Fusion (L-PBF) in as-built and heat-treated conditions (solution annealing 1,177°C/2,150°F for 15 minutes, followed by water quench) evaluated at room temperature and at high temperature (815°C/1,500°F).
Mechanical properties, metric units Condition Direction Yield strength (Rp0.2), MPa Tensile strength (Rm), MPa E-modulus, GPa Elongation (A), % Impact toughness, J As built Horizontal 627 820 194 31 105 As built Vertical 522 684 171 41 156 Heat treated Horizontal 444 770 227 40 156 Heat treated Vertical 390 637 194 52 194 As built (tested at 815 °C) Vertical 212 292 110 21 - Tensile properties in heat-treated condition, imperial units Condition Direction Yield strength (Rp0.2), ksi Tensile strength (Rm), ksi E-modulus, ksi Elongation (A), % Impact toughness, Ft.lbs As built Horizontal 91 119 28,137 31 77 As built Vertical 76 99 24,802 41 115 Heat treated Horizontal 64 112 32,924 40 115 Heat treated Vertical 57 92 28,137 52 143 As built (tested at 1,500 °F) Vertical 31 42 15,954 21 - Hardness
Typical Vickers Hardness levels (ASTM E92, ISO 6507-1, JIS Z2244, GB/T 4340.1) as well as HRC values of Osprey® H-X material in the Laser - Powder Bed Fusion (L-PBF) in as-built and heat-treated conditions.
Hardness in as-built and heat-treated condition Condition HV HRC As built 245 23 Heat treated 208 16 -
Testing
All Osprey® metal powders are supplied with a certificate of analysis containing information on the chemical composition and particle size distribution. Information on other powder characteristics is available upon request.
-
Packaging
A wide range of packaging options are available, from 1 kg (2.2 lb) to 200 kg (440 lb)*.
Contact our team who can support you with selecting the right packaging for your product and application.
*Some packaging options may not be available for all products due to international shipping regulations.
Disclaimer: Data and recommendations are for guidance only, and the suitability of a powder for a specific process or application can be confirmed only when we know the actual conditions. Continuous development may necessitate changes in technical data without notice. This datasheet is only valid for Osprey® powder.
Osprey® Online
Buy Osprey® H-X for additive manufacturing from our online store, available directly from stock.
Range of superalloys
| Osprey® | Standards* | Ni | Fe | C | Cr | Mo | Al | Ti | Nb | Co | B | Mn | Si | P | S | Other | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 625 | UNS N06625 | 58.0 min | ≤5.0 | ≤0.1 | 20.0-23.0 | 8.0-10.0 | ≤0.4 | ≤0.4 | 3.15-4.15 (Nb+Ta) | ≤1.0 | - | ≤0.5 | ≤0.5 | ≤0.015 | ≤0.015 | - |
625
|
| 713C | UNS N07713 | Bal. | ≤2.5 | 0.08-0.20 | 12.0-14.0 | 3.8-5.2 | 5.0-6.5 | 0.5-1.0 | 1.8-2.8 | - | 0.05-0.15 | - | - | - | - | Zr 0.05-0.15 |
713C
|
| 718 | UNS N07718 | 50.0–55.0 | Bal. | ≤0.08 | 17.0-21.0 | 2.80-3.30 | 0.20-0.80 | 0.65-1.15 | 4.75-5.50 | ≤1.00 | ≤0.006 | ≤0.35 | ≤0.35 | ≤0.015 | ≤0.015 | Cu ≤0.30 |
718
|
| 80A | UNS N07080 | Bal. | ≤3.0 | ≤0.10 | 18.0-21.0 | - | 1.0-1.8 | 1.8-2.7 | - | ≤2.0 | ≤0.008 | ≤1.0 | ≤1.0 | - | ≤0.015 | Cu ≤0.2, Zr ≤0.15, Pb ≤0.003 |
80A
|
| 90 | UNS N07090 | Bal. | ≤1.5 | ≤0.13 | 20.0 | - | 1.0-2.0 | 2.0 | - | 18.0 | - | - | - | - | - | - |
90
|
| H-X | UNS N06002 | Bal. | 18 | ≤0.15 | 21.0 | 9.0 | - | - | - | 1.0 | ≤0.008 | ≤0.1 | ≤0.1 | ≤0.015 | ≤0.015 | W 0.7 |
* Information about more standards is available in the datasheet for the respective alloy.